Tensile Properties of High Strength Steel Sheet with Low Yield Ratio under Impact Loading
Author(s): 
Pages: 59-63
Year: Issue:  5
Journal: BAOSTEEL TECHNOLOGY

Keyword:  高强钢马氏体形貌拉伸断裂;
Abstract: 通过室温下的仪器化冲击试验和静态拉伸试验,研究一种低屈服比高强度钢板在冲击载荷下的力学性能和断裂机理.结果表明:试验钢的组织由细小岛状马氏体与针状铁素体为主构成,马氏体体积分数为27.6%.与静态拉伸性能相比,在名义应变速率为100 s-1的冲击载荷作用下,试验用钢屈服强度提高31.6%,延伸率不降低.在静态和动态载荷下,该钢均以显微空洞长大聚集的方式发生韧性断裂,但显微空洞的形核和长大方式不同.在静态载荷下,显微空洞形核于颈缩区的铁素体晶粒内部或铁素体-马氏体两相界面处,空洞主要通过两相界面的脱开而形成长大;在动态载荷下,显微空洞主要形核于颈缩区的两相界面处,空洞主要通过马氏体粒子的开裂而形成长大.